A conveying line that runs clean for a year and then starts throwing dust is usually blamed on the resin. Most of the time the resin is the same lot it always was, and something in the route changed. Vacuum conveying generates fines in three places: at the pickup, along the pipe, and inside the receiver. Fines that arrive with the material are a fourth source, and no amount of tuning removes them. Tell those four apart before touching a setting, because the fix for one does nothing for the others.

The single biggest lever is air velocity at the pickup, and the useful number is not the blower rating but the actual pickup velocity, which depends on how far the material has to travel and how much air the line leaks.

Fines come from four places, and only three are yours

Incoming resin carries dust from the supplier, from regrind, and from drying. Virgin pellets straight from a sealed bag are typically under 0.1% fines by weight (often <500 ppm); a regrind blend can run several percent depending on screen size and how many times the material has been through the granulator. That fraction is already in the hopper before the loader starts.

The other three are created by the conveying itself. Pellets abrade against each other and against the pipe wall wherever they move fast, hit a bend at an angle, or get dragged along the bottom of a horizontal run. A vacuum line that is starved of air, or one that is oversized and running at high velocity to move a light load, both do damage — for opposite reasons.

Velocity is the number that decides how much you make

Pellets need enough air to stay suspended and enough dilution to arrive intact. Dilute-phase vacuum conveying of plastic pellets commonly runs at pickup velocities around 15–25 m/s. Below roughly 12 m/s, material starts to settle in horizontal runs and slugs through the line, which produces its own breakage at every restart. Above about 30 m/s, pellet-to-wall impact energy climbs fast and fines generation with it.

Velocity is inversely proportional to the square of pipe diameter for a given airflow, which is why stepping down a pipe size or boosting blower speed for a longer route can quietly spike velocity if nobody checks. The number that matters is at the pickup, not at the blower, because air expands under vacuum and leaks along the run.

A worked example: what a long route does to a short line

Take a 50 mm line moving 800 kg/h of polyethylene pellets at a bulk density of about 0.55 kg/L over a 30 m horizontal run with four bends. That is roughly 1.45 m³/h of bulk solids, and at a solids-to-air mass ratio of about 5.6:1 the line needs around 120 m³/h of free air, which at 50 mm bore gives a pickup velocity around 17 m/s. Comfortable.

Now relocate the source and add 40 m of run and four more bends. Same pipe, same blower, same 800 kg/h. The extra length adds pressure drop, the airflow at the pickup falls toward 85 m³/h, and velocity drops toward 12 m/s. Material starts to settle in the horizontals, the line slugs, and someone replaces the blower or opens the air bleed and boosts speed to clear it. If airflow is pushed to 180–200 m³/h on that 50 mm pipe, velocity reaches 25–28 m/s (and even higher near the receiver as air expands under deeper vacuum) while the pellets hit eight bends instead of four. Fines go up at both ends of the adjustment.

The fix is not a bigger blower. It is either a larger bore to carry the same mass at lower velocity, a shorter route, or a receiver and control cycle that matches the new pressure drop. Those are route decisions, not settings.

The pickup and the receiver each have a job

At the source, an immersion tube set too deep buries itself in the material and pulls pellets through the inlet at high velocity with no air cushion. Set too shallow, it sucks air and starves the line. The usual starting point is an immersion depth of roughly half the material bed, adjusted so the inlet stays covered through the drawdown without dragging on the bin floor. A sharp or damaged inlet edge abrades pellets on the way in.

At the receiver, the separation stage is what keeps fines out of the vacuum pump and out of the next machine. A filter that is loading up increases pressure drop and reduces airflow, while a torn, bypassed, or too-coarse screen passes fines into the blower line. Collected fines need a defined removal interval, not a cleaning when somebody notices the airflow has fallen off. Across our factory in Zhongshan and our manufacturing partners, KYSHIN supplies central material conveying systems configured around the route and material data for each project, and the receiver and central material filter are chosen as part of that package rather than bolted on afterward.

Where fines collect tells you which problem you have

Walk the route from source to machine and note where material turns up during cleaning. Fines settle at elbows, in horizontal runs, at flexible hose sections, at diameter changes, and at the receiver inlet. A single recurring location points to a route condition — a tight-radius bend, a sagging hose, a step in pipe size — rather than a material problem.

If the same bend fills up every week after cleaning, the bend is the cause. If fines appear evenly along a long horizontal run, the velocity is too low and material is dragging. If the receiver filter loads quickly but the pipe is clean, the separation stage is undersized for the material form, which is common when a line designed for pellets starts running flake or regrind.

The comparison that settles it is a sample at the source and a sample at the receiver, same grade and same lot. Fines that increase along the route are created by conveying. Fines already present at the source come from resin supply, the granulator, or the dryer, and a conveying change will not fix them. Our vacuum receivers and detachable receiver loaders are specified against the material form for exactly this reason.

What we cannot decide for you

The acceptable fines level is set by your resin supplier and your quality process, not by the conveying equipment. A glass-filled grade, a soft elastomer, and a clear polycarbonate for optical parts all tolerate different amounts of dust, and a number that is fine for one is a defect source for another. We can size a line to keep velocity in a sensible band for a given material and route; we cannot tell you what your customer will accept in the molded part. That limit has to come from your side.

One more limit worth stating plainly: a line that was sized correctly for its original route is not automatically correct after a relocation, an added machine, or a switch to regrind. The route data changed, so the pickup, vacuum unit, receiver, and control cycle need to be checked as one package. That is the review we do when a customer sends a route drawing and the locations where fines keep appearing.

If fines keep coming back at the same point after cleaning, send the resin grade, the particle form, the route length and lift, the bend count, and the observed locations. That is enough to tell whether the line is being asked to do something it was not built for.

Inspection that means opening a receiver, pulling hose, or working near a live vacuum point follows the machine manual and your plant's isolation procedure, with qualified personnel on the electrical and pressure side.