A masterbatch pellet that measures 3 mm across and one that measures 1.5 mm can both be "2 % black." Put them through the same volumetric auger at the same dial setting and you will not get 2 % twice. The screw counts volume. Your recipe is written in weight. Pellet size and bulk density are what sit between those two units, and most color-shift investigations that stall for a week are really a units mismatch nobody wrote down.

This page is about closing that gap: what to weigh, how to run the comparison, and where a weight-based blender earns its price.

The screw doses volume, the recipe asks for mass

A volumetric masterbatch feeder delivers a fixed volume per revolution. Mass per unit volume is bulk density, and bulk density is a packing property, not a chemistry property. Change the pellet shape and the same auger setting delivers a different mass.

The spread is bigger than most people expect. Free-flowing masterbatch pellets commonly bulk somewhere between 0.55 and 0.85 kg/L, and the same compound in a different pellet geometry can land at either end. At 0.60 kg/L an auger moving 0.5 L/h delivers 300 g/h. The identical setting on 0.80 kg/L material delivers 400 g/h — a third more colorant, from a lot change and nothing else.

That is the whole reason pellet size matters at the screw. It is not a resin question. It is whether the dosing device is counting volume or counting mass.

Measure bulk density before you touch the setting

You need one number per material, and it takes five minutes. Fill a 1 L graduated container from a fixed height, level it without tamping, and weigh the contents, then divide grams by 1000 for kg/L. Three repeats averaged together will show you how free-flowing the material is.

Measure virgin, regrind, and the masterbatch itself. Regrind is where the number usually surprises people, because a granulator produces a wide particle distribution and fines pack into the gaps between bigger pieces. A 30 % regrind addition can shift the blend's bulk density by 10 % or more depending on the screen and the knife condition.

Two cautions on the measurement. Tapped or settled material reads higher than material as it flows through a hopper, so do not vibrate the container. And if your incoming check and your supplier's data sheet disagree by more than about 10 %, check whether one of you is quoting tapped density — they are different tests and will never match.

A worked comparison you can run in an afternoon

Take a press running a 400 g shot on a 35-second cycle. That is about 41 kg/h of total throughput. At a 2 % letdown the masterbatch demand is roughly 0.82 kg/h, or 820 g/h.

Set the volumetric doser to deliver that and run twenty timed catches, converting each catch weight to an equivalent hourly rate in g/h. Suppose the twenty readings average 790 g/h with a high of 850 and a low of 730. The average is 4 % under target and the spread is 15 % of the mean.

Now change only the masterbatch lot, keep the dial where it is, and repeat the timed catches. If the new average lands at 880 g/h, the feeder is responding to volume: the new lot packs denser, the auger scoops more mass per turn, and the colorant load just went up 11 % with nobody touching a setting. If the average holds near 790 g/h but the spread widens, the problem is flow stability rather than density, and you are looking at bridging, auger wear, or a hopper that is running too empty.

That distinction — average versus spread — is the part most troubleshooting skips. A density shift moves the average. A flow problem moves the spread. They have different fixes.

What gravimetric batching actually removes

A weight-based blender closes the loop the volumetric doser leaves open. It weighs each component as it dispenses, so a denser lot is caught by the scale rather than passed through to the melt. The Gravimetric Blender Series arranges multi-bin recipes and mixes in an integrated chamber, and for a plant chasing pellet-size variation that is the direct answer: the volume assumption disappears at the dosing step.

It is not a cure for everything, and this is where we are honest about scope. A gravimetric blender will report the weight correctly and still deliver the wrong recipe if the screw is worn, if the letdown ratio was entered wrong, or if regrind carries a particle distribution so wide that the blender's small weigh hopper cannot sample it representatively. Weight control fixes density variation. It does not fix a worn feed screw or a bad ratio.

Where a single colorant is the only additive, a single-component masterbatch doser is often the right size of tool, and a twin-hopper color masterbatch doser covers two components without going to a full gravimetric frame. Across our Zhongshan factory and our manufacturing partners, we build and supply across these categories, and the choice between volumetric and gravimetric usually comes down to how tight the color tolerance is and how often lots change.

Sizing inputs we need before quoting a blender

When a plant asks us to configure weight-based batching, four numbers decide the machine and one of them is routinely missing.

The material list and recipe percentages set the bin count and the ratio range. Total hourly demand sets the throughput. The minimum component ratio matters more than people think: a 0.5 % additive on a 50 kg/h line is 250 g/h, and a weigh hopper sized for 5 kg batches (where a 0.5 % dose is only 25 g per batch) will struggle to resolve that drop to better than a few percent. And bulk density for every component sets hopper volume — 25 kg of a 0.55 kg/L masterbatch needs about 45 L of working volume, while the same mass of a 0.85 kg/L material needs 29 L.

Gather those four and a configuration conversation takes one call. Skip the bulk densities and we are guessing at hopper sizes, which is exactly the guessing this page is trying to remove.

When the feeder checks out and the color still drifts

If a timed weigh confirms the doser is delivering what it should, and a lot swap does not move the average, stop looking at the feeder. The next candidates are downstream. A worn check ring lets melt slip back during injection, shot weight wanders, and the colorant-to-resin ratio moves with it even though the doser never changed. Barrel and screw wear does the same thing more slowly. Neither shows up on a feeder calibration record.

The other common cause is proportioning at the wrong point. Masterbatch added at the machine throat mixes differently from masterbatch compounded into the pellet, and a short, low-compression screw may not distribute a high-loading colorant evenly no matter how accurately it was weighed. That is a screw design conversation, not a dosing one.

Lock out and isolate any equipment before internal inspection, and leave electrical and mechanical work to qualified personnel. The weigh checks come first because they are cheap, they need no tools beyond a scale and a stopwatch, and they eliminate the dosing step before anyone opens a barrel.

If you have the material list, the ratios, the hourly demand and the measured bulk densities, send them through the mixing and dosing category page and we will work out whether a gravimetric frame or a single-component doser fits the line.